RHS 180×100×10 is an RHS Hot-finished section from the UK Blue Book (SCI P363); RHS 175×100×12.7 is the closest equivalent in the European (Continental) range. They are close to interchangeable in bending: 288 cm³ against 288 cm³ of plastic modulus, a difference of 0.0%. RHS 180×100×10 is the lighter of the two at 40 kg/m against 47.3 kg/m, a saving of 15.4% on steel weight. RHS 180×100×10 is deeper, 180 mm against 175 mm, which matters where the floor zone is tight.

Section properties side by side. Bold marks the more favourable value where one is.
PropertyRHS 180×100×10
RHS Hot-finished
RHS 175×100×12.7
RHS Cold-formed
Difference
Mass40 kg/m47.3 kg/m-15.4%
Depth180 mm175 mm+2.9%
Width100 mm100 mmsame
Web thickness0 mm0 mmsame
Flange thickness0 mm0 mmsame
Area50.9 cm²56.5 cm²-9.9%
Second moment, major (Iy)2,040 cm⁴1,867 cm⁴+9.3%
Plastic modulus, major (Wpl,y)288 cm³288 cm³same
Elastic modulus, major (Wel,y)226 cm³213 cm³+6.1%
Second moment, minor (Iz)787 cm⁴777 cm⁴+1.3%
Plastic modulus, minor (Wpl,z)188 cm³195 cm³-3.6%
Radius of gyration, minor (iz)3.93 cm3.71 cm+5.9%
Torsion constant (It)1,860 cm⁴2,052 cm⁴-9.4%

RHS 180×100×10 to BS EN 10210-2:2006; RHS 175×100×12.7 to EN 10219 · Continental Steel. Difference is expressed relative to RHS 175×100×12.7.

How to choose between them

On stiffness, RHS 180×100×10 has the larger second moment of area: 2,040 cm⁴ against 1,867 cm⁴, a difference of 9.3%. This matters more often than the strength comparison, because on normal floor spans deflection rather than bending capacity sets the beam size - so if the two are close on modulus but apart on inertia, the stiffer one is usually the better answer even when it is not the stronger one.

Measured as bending capacity per kilogram of steel, RHS 180×100×10 is the more efficient section: 7.2 against 6.1 cm³ per kg/m, 18.2% better. Over a floor of repeated beams that difference is real tonnage, though it is often outweighed by whichever section the fabricator can actually source.

These come from different catalogues, so treat the swap as a design change rather than a like-for-like substitution. RHS Hot-finished sections are specified to BS EN 10210-2:2006 and RHS Cold-formed to EN 10219 · Continental Steel; the steel grades, tolerances and available lengths differ, connection details and bolt gauges are set out differently, and the two are rarely both stocked in the same market. Check availability before changing a section on a drawing to save 15.4% weight.

In short, RHS 175×100×12.7 is the stronger section and RHS 180×100×10 is the lighter one; where those are the same section, it is the clear choice, and where they are not, decide on whether your design is governed by capacity or by tonnage.

Common questions

They are effectively equal in bending. RHS 180×100×10 has a plastic modulus of 288 cm³ and RHS 175×100×12.7 has 288 cm³, a difference of only 0.0% - within the margin that section choice normally turns on. Compare stiffness and availability instead.

RHS 180×100×10 at 40 kg/m, against 47.3 kg/m for the other - a saving of 15.4%. Over a repeated floor beam that is a real cost difference, but check it against the deflection case before taking it.

Structurally it is the closest equivalent we hold: RHS 175×100×12.7 gives 288 cm³ of plastic modulus and 1,867 cm⁴ of inertia against 288 cm³ and 2,040 cm⁴. But they are from different catalogues (BS EN 10210-2:2006 and EN 10219 · Continental Steel), so this is a design change, not a drop-in swap: re-check deflection, connection detailing and local availability.

RHS 180×100×10, with a second moment of area of 2,040 cm⁴ against 1,867 cm⁴ (9.3% more). Deflection under a uniform load goes as 5wL⁴/384EI, so it is inversely proportional to I - on a span where the deflection limit governs rather than strength, this is the number that decides the section.