RHS 200×100×7.1 vs RHS 200×100×8
RHS 200×100×7.1 is an RHS Hot-finished section from the UK Blue Book (SCI P363); RHS 200×100×8 is the closest equivalent in the European (Continental) range. RHS 200×100×8 carries more bending: 267 cm³ of plastic modulus against 254 cm³, 4.9% more. RHS 200×100×7.1 is the lighter of the two at 31.4 kg/m against 33.9 kg/m, a saving of 7.4% on steel weight. Both are about 200 mm deep, so either fits the same construction zone.
| Property | RHS 200×100×7.1 RHS Hot-finished | RHS 200×100×8 RHS Cold-formed | Difference |
|---|---|---|---|
| Mass | 31.4 kg/m | 33.9 kg/m | -7.4% |
| Depth | 200 mm | 200 mm | same |
| Width | 100 mm | 100 mm | same |
| Web thickness | 0 mm | 0 mm | same |
| Flange thickness | 0 mm | 0 mm | same |
| Area | 40 cm² | 43.2 cm² | -7.4% |
| Second moment, major (Iy) | 2,020 cm⁴ | 2,091 cm⁴ | -3.4% |
| Plastic modulus, major (Wpl,y) | 254 cm³ | 267 cm³ | -4.9% |
| Elastic modulus, major (Wel,y) | 202 cm³ | 209 cm³ | -3.3% |
| Second moment, minor (Iz) | 674 cm⁴ | 705 cm⁴ | -4.4% |
| Plastic modulus, minor (Wpl,z) | 155 cm³ | 165 cm³ | -6.1% |
| Radius of gyration, minor (iz) | 4.1 cm | 4.04 cm | +1.5% |
| Torsion constant (It) | 1,630 cm⁴ | 1,811 cm⁴ | -10.0% |
RHS 200×100×7.1 to BS EN 10210-2:2006; RHS 200×100×8 to EN 10219 · Continental Steel. Difference is expressed relative to RHS 200×100×8.
How to choose between them
On stiffness, RHS 200×100×8 has the larger second moment of area: 2,091 cm⁴ against 2,020 cm⁴, a difference of 3.4%. This matters more often than the strength comparison, because on normal floor spans deflection rather than bending capacity sets the beam size - so if the two are close on modulus but apart on inertia, the stiffer one is usually the better answer even when it is not the stronger one.
Measured as bending capacity per kilogram of steel, RHS 200×100×7.1 is the more efficient section: 8.1 against 7.9 cm³ per kg/m, 2.7% better. Over a floor of repeated beams that difference is real tonnage, though it is often outweighed by whichever section the fabricator can actually source.
These come from different catalogues, so treat the swap as a design change rather than a like-for-like substitution. RHS Hot-finished sections are specified to BS EN 10210-2:2006 and RHS Cold-formed to EN 10219 · Continental Steel; the steel grades, tolerances and available lengths differ, connection details and bolt gauges are set out differently, and the two are rarely both stocked in the same market. Check availability before changing a section on a drawing to save 7.4% weight.
In short, RHS 200×100×8 is the stronger section and RHS 200×100×7.1 is the lighter one; where those are the same section, it is the clear choice, and where they are not, decide on whether your design is governed by capacity or by tonnage.